Add to Cart
Custom Made Titanium Wire For Titanium Products Space Metal
Titanium is a metal element, titanium melting point 1660℃, boiling point 3287℃, density 4.54g/cm³. Titanium is a gray transition metal, characterized by its light weight, high strength and good corrosion resistance. Because of its stable chemical properties, good resistance to high temperature, low temperature, strong acid, strong alkali, as well as high strength, low density, is known as "space metal".
The two most prominent advantages of titanium are high specific strength and corrosion resistance, which determines the application of titanium in aerospace, weaponry, energy, chemical, metallurgy, construction and transportation fields.
Item | Titanium wire |
Material | Pure Titanium and alloy |
Grade | GR1 GR2 GR3 GR4 GR5 GR7 GR9 GR12 |
Standard | GB,ASTM, BS, BSW, ISO ASTM B863 ASTM B348 ASTM F67 ASTM F136 |
Size | Dia(0.06--6) *L |
Specification | Dia 0.03-6.0mm |
Certification | ISO9001:2008 |
MOQ | 5 kilograms |
Process | Bar billets-hot rolling-drawing-annealing-strength-pickling |
Surface | Polishing, picking, acid washed, black oxide |
Type | Straight , spool ,coil |
Application | Welded wire, welded wire, glasses etc |
Wire Gauge | 0.1-8.0mm |
Type | Straight, Coil, Spool |
Surface Treatment | Pickling Polished |
Application | Chemical equipment, such as pipes, heat exchangers, evaporators, heaters, reaction kettles etc. |
Chemical Composition
Grade | N | C | H | Fe | O | Al | V | Pa | Mo | Ni | Ti |
Gr1 | 0.03 | 0.08 | 0.015 | 0.2 | 0.18 | / | / | / | / | / | bal |
Gr2 | 0.03 | 0.08 | 0.015 | 0.3 | 0.25 | / | / | / | / | / | bal |
Gr3 | 0.05 | 0.08 | 0.015 | 0.3 | 0.35 | / | / | / | / | / | bal |
Gr4 | 0.05 | 0.08 | 0.015 | 0.5 | 0.4 | / | / | / | / | / | |
Gr5 | 0.05 | 0.08 | 0.015 | 0.4 | 0.2 | 5.5~6.75 | 3.5~4.5 | / | / | / | bal |
Gr7 | 0.03 | 0.08 | 0.015 | 0.3 | 0.25 | / | / | 0.12~0.25 | / | / | bal |
Gr9 | 0.03 | 0.08 | 0.015 | 0.25 | 0.15 | 2.5~3.5 | 2.0~3.0 | / | / | / | bal |
Gr12 | 0.03 | 0.08 | 0.015 | 0.3 | 0.25 | / | / | / | 0.2~0.4 | 0.6~0.9 | bal |
Tensile Requirements
Grade | Tensile strength(min) | Yield Strength(min) | Elongation(%) | ||
ksi | MPa | ksi | MPa | ||
Gr1 | 35 | 240 | 20 | 138 | 24 |
Gr2 | 50 | 345 | 40 | 275 | 20 |
Gr3 | 65 | 450 | 55 | 380 | 18 |
Gr4 | 80 | 550 | 70 | 483 | 15 |
Gr5 | 130 | 895 | 120 | 828 | 10 |
Advantages:
1.Low Density and High Strength
2.Excellent Corrosion Resistance
3.Good resistance to high temperature
4.Excellent Bearing to cryogenic property
5.Good thermal properties
6.Low Modulus of Elasticity
7.Toughness, light weight
8.High property of acid and alkali resistance